Relay-Version: version B 2.10 5/3/83; site utzoo.UUCP Posting-Version: version B 2.10 5/3/83; site utcsrgv.UUCP Path: utzoo!utcsrgv!spoo From: spoo@utcsrgv.UUCP (Suk Lee) Newsgroups: net.audio Subject: Re: To Dust or Not To Dust Message-ID: <2970@utcsrgv.UUCP> Date: Mon, 19-Dec-83 04:34:59 EST Article-I.D.: utcsrgv.2970 Posted: Mon Dec 19 04:34:59 1983 Date-Received: Mon, 19-Dec-83 05:30:24 EST References: <347@whuxk.UUCP> <129@watrose.UUCP> Organization: CSRG, University of Toronto Lines: 10 In the "good old days" (I wasn't there), static buildup on voltmeter faces was avoided by coating the surface with a *THIN* film of liquid detergent and letting it air-dry. More easily, there are various anti-static sprays meant for records that work just as well on plexiglass covers. From the pooped paws of: Suk Lee ..!{decvax,linus,allegra}!utzoo!utcsrgv!spoo